Infrared optics · Materials and processes
Five infrared materials, with forming, grinding, single-point turning and coating
OOTEE Optics fabricates germanium, silicon, chalcogenide glass, ZnSe and ZnS lenses for infrared optical systems. Depending on the material, surface form and drawing, we select forming, grinding and polishing or single-point diamond turning, with AR coating, DLC protective coating and optical inspection in support.
Each figure applies to a specific material, process and part condition; it does not mean all maximum values are reached simultaneously at the largest aperture.
Infrared lens fabrication is not only about controlling diameter and thickness: the optical surface must meet the designed shape, and the two surfaces must keep the specified relationship to each other and to the mechanical datums. Different parts call for different process combinations:
Establish the blank outline and preliminary curve, leaving stock for finishing.
Progressively correct the optical surface, controlling figure error and surface defects.
Generate the optical surface through precise machine motion and tool path, suited to aspheric and diffractive needs of the relevant material.
Configure AR, protective or reflective coatings for the working band and environment.
Check dimensions, figure, centration and spectral performance to form the acceptance basis against the drawing.
Drawing and material review → blank preparation / forming → grinding or single-point turning → dimension and figure inspection → coating → final review
A part usually cycles between processes: figure is re-measured after polishing, spectra after coating. A deviation in any step is carried into the next.
Aperture ranges are listed per material and process; the main selection basis is the material plus process combination.
| Material | Grinding & polishing aperture | Single-point turning aperture | Focus on this page |
|---|---|---|---|
| Germanium (Ge) | φ4–200 mm | φ4–300 mm | Lens fabrication with AR and AR+DLC |
| Silicon (Si) | φ4–200 mm | φ4–200 mm | Lens fabrication with 3–5 μm coating |
| Chalcogenide glass | φ4–140 mm | φ4–180 mm | Forming, grinding, turning and coating |
| Zinc selenide (ZnSe) | φ4–200 mm | φ4–200 mm | Lens fabrication with AR coating |
| Zinc sulfide (ZnS) | φ4–200 mm | φ4–200 mm | Lens fabrication with AR coating |
Material choice must match the optical design, working band, ambient temperature and mounting conditions. The same material in a different grade, thickness or process route may support different tolerances and coating conditions. Please specify the grade and the drawing.
Chalcogenide coating data covers grades such as IRG201, IRG202, IRG204, IRG205 and IRG206, shown here as material and coating matching guidance; machinability of a given grade depends on the blank condition.
Depending on the chalcogenide blank and lens geometry, we establish the part outline by cutting, rough blank moulding and milling, preparing it for grinding or single-point processing. Rough blank moulding here is a forming step and is not equivalent to precision moulding of the final optical surface.

| Item | Capability listed | Inspection |
|---|---|---|
| Aperture range | φ4–200 mm | Per dimensional inspection requirements |
| Radius deviation | ±0.002 mm | Interferometer |
| Center thickness deviation | ±0.005 mm | Micrometer |
| Diameter deviation | ±0.002 mm | Laser diameter gauge |
| Surface quality | 80-50 | Visual inspection |
| Surface figure PV | 0.8–1.5 μm | Interferometer |
The forming stage is mainly about blank dimensions, curvature and finishing stock. Its figure and surface quality should be listed separately from final finishing values so customers can judge the delivery state of each step.
Depending on material and part geometry we use high polishing, low polishing or double-side polishing. Grinding and polishing must control surface shape while respecting center thickness, diameter and downstream assembly requirements.

| Item | Chalcogenide | Germanium | Silicon | ZnSe / ZnS |
|---|---|---|---|---|
| Aperture range | φ4–140 mm | φ4–200 mm | φ4–200 mm | φ4–200 mm |
| Radius deviation | ±0.002 mm | ±0.002 mm | ±0.002 mm | ±0.002 mm |
| Center thickness deviation | ±0.005 mm | ±0.005 mm | ±0.005 mm | ±0.005 mm |
| Diameter deviation | ±0.002 mm | ±0.002 mm | ±0.005 mm | ±0.002 mm |
| Surface quality grade | 40-20 to 80-50 | 40-20 to 80-50 | 40-20 to 80-50 | 40-20 to 80-50 |
| Surface figure PV | 0.1–0.6 μm | 0.1–0.6 μm | 0.1–0.6 μm | 0.1–0.6 μm |
The ranges describe assessable capability. Acceptance values for a specific part depend on material, aperture, curvature, thickness and the effective inspection aperture.
Single-point diamond turning generates the designed surface through precise relative motion between tool and workpiece. For aspheres the tool path is defined from curvature, conic constant and aspheric coefficients; for diffractive surfaces the structure parameters and inspection requirements must also be defined.

| Item | Chalcogenide | Germanium | Silicon | ZnSe / ZnS |
|---|---|---|---|---|
| Aperture range | φ4–180 mm | φ4–300 mm | φ4–200 mm | φ4–200 mm |
| Radius deviation | ±0.002 mm | ±0.002 mm | ±0.002 mm | ±0.002 mm |
| Center thickness deviation | ±0.005 mm | ±0.005 mm | ±0.005 mm | ±0.005 mm |
| Diameter deviation | ±0.002 mm | ±0.002 mm | ±0.005 mm | ±0.002 mm |
| Surface quality grade | 60-40 to 80-50 | 40-20 to 80-50 | 40-20 to 80-50 | 40-20 to 80-50 |
| Surface figure PV | 0.1–0.6 μm | 0.1–0.6 μm | 0.1–0.6 μm | 0.1–0.6 μm |
| Machine | Throughput | Qty |
|---|---|---|
| Single-point diamond lathe LK100 | 5000 mm / day | 3 |
| Single-point diamond lathe L200 | 8000 mm / day | 1 |
The table below is the general tolerance basis, used to judge whether a requirement calls for a dedicated process route; it is not mixed with the per-material tables above.
| Item | Standard | High precision (reference) |
|---|---|---|
| Diameter tolerance | 0.01–0.03 mm | 0.003–0.005 mm |
| Surface quality | 60-40 / 80-50 | 40-20 |
| Thickness tolerance | ±0.03 mm | ±0.005 mm |
| Power N | 3–5 | 0–1 |
| Irregularity ΔN | 0.5–1 | 0.2–0.3 |
| Sagitta tolerance | ±0.03 mm | ±0.005 mm |
| Radius range | R5–R∞ | R5–R∞ |
| Aspheric figure error | 0.5–1 μm | 0.1–0.2 μm |
Diameter tolerance must be stated with upper and lower deviation on the drawing; power, irregularity and aspheric figure should be accompanied by test wavelength, effective aperture and evaluation method. High-precision values are confirmed per part and are not a blanket guarantee for all materials and sizes.
The general φ5–260 mm range describes the applicable production window; the main table on this page uses material-plus-process apertures so it is not confused with figures such as φ300 mm for germanium single-point turning.
AR coatings reduce surface reflection loss in a specified band; DLC diamond-like carbon coatings suit applications with surface durability requirements. Different coating designs affect transmission, reflection and environmental behaviour differently, so they are chosen against the actual application.
| Substrate | Coating / band | Average transmission |
|---|---|---|
| Germanium | Dual-side AR, 8–12 μm | ≥97% |
| Germanium | 4–12 μm coating design | approx. 96% |
| Silicon | 3–5 μm coating design | approx. 98% |
| Germanium | AR+DLC, 8–12 μm | ≥91% |
| Silicon | AR+DLC, 3–5 μm | ≥85% |
| Chalcogenide | 8–12 μm or 8–14 μm, per grade and design | ≥96% |
| ZnSe | AR coating | Per band and drawing |
| ZnS | AR coating | Per band and drawing |
Each curve corresponds to one substrate, one band and one coating design and cannot stand for the whole product range; delivered parts are accepted against measured curves from the same batch.




Figures reflect current capability. Each product must state substrate grade, thickness, single or dual-side stack, angle of incidence and measurement conditions; "approx. 96%" and "approx. 98%" remain approximate and are not minimum guaranteed values.
Equipment counts reflect the present production line and describe process coverage, not a per-piece capacity commitment.
| Process | Machine and model | Qty |
|---|---|---|
| Forming | Centering machine SPCM-M1 | 5 |
| Forming | CNC lathe | 2 |
| Forming | Rough blank moulding furnace | 5 |
| Grinding | Four-axis tilt machine HT120.4DF | 2 |
| Grinding | Push-pull machine LP-4NP | 5 |
| Grinding | Upper lapping machine ZHB-8 | 10 |
| Grinding | Lower lapping machine | 10 |
| Grinding | Six-axis tilt machine HT120.6DF | 2 |
| Grinding | Single-axis / chamfering machine ZKM05A | 5 |
| Grinding | Low polishing machine QJP25.4B | 4 |
| Single-point turning | Single-point diamond lathe LK100 / L200 | 4 |
| Inspection | Equipment | Note / wavelength range |
|---|---|---|
| Surface figure | Multiple interferometers (Fuji 601, SD-60, G150-2, AC150 and others) | Figure assessed per part and inspection setup |
| Profile | PGI profilometer | Curved and aspheric profile checks |
| Centration | TC-1 and other centering stations | Relationship between optical and mechanical datums |
| Spectrophotometry | LAMBDA950 spectrophotometer | 190–3300 nm |
| Reflectance | MSP-108P reflectometer | 390–1050 nm |
| IR spectroscopy | SPECTO-TWO FTIR | 1400–20000 nm (1.4–20 μm) |
| Spectrophotometry | Xinrui UV-IR photometer | 200–1100 nm |
An instrument wavelength range does not mean the same inspection accuracy is reached for every material and accessory configuration. Final inspection items must correspond to the actual drawing and test conditions.
On one drawing, several values constrain each other. Understand the scope of each term before discussing feasibility.
Outer diameter is for mechanical assembly; the clear aperture is the region where optical performance must be guaranteed. Clamping, chamfer and edge zones may not count as clear aperture and should be marked separately on the drawing.
Radius describes how strongly a spherical surface curves. An asphere additionally needs conic constant, higher-order coefficients, axis orientation and aperture — one R value cannot define manufacturing. R∞ is commonly used for a flat.
Center thickness is the separation of the two surfaces at the defined center point; sagitta is the height of a curved surface relative to a stated datum. They control different geometry and cannot substitute for each other.
PV is the difference between the maximum and minimum error relative to the agreed reference or design surface. State the effective inspection aperture, fitting method and terms excluded. Figure PV describes shape error and is not surface roughness.
These grades describe scratch and dig requirements and must be used with an agreed inspection standard, illumination and judgement method. They cannot be converted directly into Ra or Rq roughness values.
Power describes the interference fringe deviation under the stated test conditions; irregularity addresses local deviation. Both must be read with the test wavelength, method and aperture — fringe counts are not micrometre values.
Centration describes deviation between optical axis, surface and mechanical datum. Angular decentration and a positional offset in micrometres are different quantities; acceptance must state the datum and measurement definition.
Machinability of an infrared part depends on the combination of material grade, geometry and inspection conditions. Define the inputs before discussing tolerances.
| Category | Details |
|---|---|
| Material | Material name, grade and material certificate requirements |
| Geometry | Outer diameter, center thickness, edge thickness, chamfer and clear aperture |
| Optical form | Flat, spherical, aspheric or diffractive definition |
| Tolerances | Figure, surface quality, thickness, centration and other tolerances |
| Operating conditions | Working band, angle of incidence, ambient temperature and mounting |
| Coating | AR, DLC, metal reflection or other stack |
| Acceptance | Inspection method, sampling plan and delivered documents |
We assess material, process, inspection and coating fit against the customer drawing and operating conditions. For prototypes and volume orders, key tolerances, process route and acceptance conditions are confirmed separately.
Deliverables can include dimensional records, figure inspection results, spectral curves, visual inspection and batch identification as agreed. Any parameter without defined test conditions is completed during technical review.
Send a drawing